Description of the article « Catalyst 3099 - Stamping »
Instructions for use : Weigh the 3% catalyst well (if not the product will polymerize in your container). Apply your first coat quickly to avoid bubbles. Then you can apply with a spatula or a brush.
Stamping catalyst for vertical application (not flowing).
Put 3% of 3099 with 3481/3483/3487.
Working time 15 minutes at 20° / Demoulding 2 hours.